Here’s the method I used if anybody could tell me where I went wrong would be highly appreciated thanks
I blasted into a baller jar and let the tane evaporate outside on its own I then whipped it up for 2 days while in the baller jar after 2 days I removed and placed into vac chamber I pumped to -28hg and released at room temperature for 3 days the oil where rising and going like a muffin shape but still sparks like mad when I put a flame to it.
My heat mat arrived this morning and I set it to 42c and placed my chamber on top of it my oil turned to a crumble type of texture the oil is now doing nothing at all inside the chamber just keeping its shape and form even on a 42c heat mat
Also if Could anybody give me a better method thanks
if you’re using can butane you might have something else in there… but you can try spreading it out thin on that piece of parchment it’s on and set back into your vac and set to 46c and let extract come up to temp for 10-20 min before pulling vac, let sit for 30 min to 1 hour scrape wax back into pile and whip, repeat until satisfied with end result.
Looks like you’re improving…presumably thanks to the advice proffered above. congrats.
However, just as creating a new user to ask your next question was not helpful (Wax/budder/sugar methods without vaccum oven), creating a new topic for the same issue (you’re new and haven’t figure out your purge) is also counterproductive.
Imagine the NEXT person looking for this information.
You’d prefer it in a nice concise package, so why deliberately spray it all over the place?
Key points 1) thin films purge better. 2) water will cause both sugaring and spitting in response to flame.
It’s much easier to end up with water in your product when open blasting….
You are not the only one on this journey, and all the questions you currently have, have almost certainly been explored before around here…if you want information on specific subjects, go find them and join the discussion by asking clarifying questions. Eg: Cured Badder Tek if that’s what you seek.
-28 doesn’t sound like you’ve got things sealed up right. Let’s see that vacuum pump.
I was not aware of this I thought I could just make threads for advice
I did not open blast into any water I open blasted straight into a mason jar and let it evaporate Outside with air it hasn’t been near water at all really
I had it in the vac chamber at uk room temperature (no heat mat) for 3 days this is how it where blowing up I will attach a pic my heat mat arrived this morning and I put my vac chamber on top with the oil inside once the mat reached 40c I pumped pumped to -28hg there was hardly any bubbling it just puffed a tiny bit after 1 hour i had hard crumble
Dew point in London today is 8C which would certainly provide enough water IN THE AIR to potentially manage some in your BHO (remind us what temp your solvent of choice boils?).
…and while we are on the subject (solvent of choice), understand that the 99.99% n-butane you’re using is almost certainly not even 90%
Bro I explained everything on one of my posts I even posted a pic of the pump I’ve looked for threads on how to purge properly etc everything is about closed loops and vac ovens I don’t have a vac oven or closed loop but will be looking to invest in one once I have funds ready I just replied to this thread like I where told to do instead of creating a new one and people are still moaning at me