All I’m saying is any sample should come as they should when in production. Otherwise I would never expect a client to come purchase. I also didn’t post this photo as it wouldn’t load with the others. But this was after loading decarbing live rosin. While still warm.
I guess loading with a heated glass syringe got a little close. User error on my fault so I proceeded the second one with a different loading process. Went fine till the whole thing tore apart with no force at all.
Just my 2¢ nothing that is heated should ever be made of plastic. Especially while working with aromatic hydrocarbons. (Yes I said it cause terpenese)
If other materials were used such as borosilicate glass or even glass I wouldn’t be opposed but there are other underlying problems.