I was interested in trying Loveland’s SST28 which claims 28% monosilicic acid. Seems like quite the value compared to something like powerSi @1%. Can anyone talk me out of this or maybe im missing something? Im currenty using Agsil16H but I like the lack of K and the stable pH of the SST. BUT…theres a chart on manicbotinx that shows it having the lowest-in-class plant available si. https://manibotanix.com/silica-additive-quality/ Do they have this wrong? It also shows mills vitilize as very low in available si but ive seen that product work well. Looks like i have some gaps in my knowledge and any input is appreciated. Thanks yall, have a good day!!
1 Like
Good thread with lots of silica talk. Even a diy option for monosilicic
Cool thanks i didnt know if i should post there or here