Shouldn’t clay be on the bottom if we think micron size?
Silica (top)
Alumina (middle)
Clay (bottom)
?
Shouldn’t clay be on the bottom if we think micron size?
Silica (top)
Alumina (middle)
Clay (bottom)
?
Clay should always be on the bottom. Whether you use T5 or Celite or generic DE.
I use w1 to replace all the other powders (t41, silica, etc) and it’s been working great.
I run around 5000g through 1000g of powder split between 2 or three runs.
I do enjoy my aluminas and silicad to be on top when I include them, but w-1 seems to be the ticket on its own in almost all cases.