Beads loaded beads molsieves or polystyrene

I am not familiar with the HHC reaction. As long as this is no issue here, try to get one of those:
CT175DR
CT269DR
CT275DR

They are just a little different in detail (inner pore size, etc.) but all did the Job.
Parameters are comparable to a regular pTSA reaction.

5 Likes